Effect of melt superheat treatment on solidification behavior and microstructure of new Ni-Co based superalloy 期刊论文
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2021, 卷号: 15, 页码: 4970-4980
作者:  Cui, Hongyang;  Tan, Yi;  Bai, Rusheng;  Li, Yi;  Zhao, Longhai;  Zhuang, Xinpeng;  Wang, Yilin;  Chen, Ziang;  Li, Pengting;  You, Xiaogang;  Cui, Chuanyong
收藏  |  浏览/下载:125/0  |  提交时间:2022/01/27
Superheat treatment  Dendritic segregation  Microstructure refinement  New Ni-Co Based superalloy  
Effect of Si on the Solidification Segregation Behavior of a New Ni-Co-Based Superalloy 期刊论文
ADVANCED ENGINEERING MATERIALS, 2021, 页码: 11
作者:  Zhuang, Xinpeng;  Tan, Yi;  You, Xiaogang;  Cui, Hongyang;  Cui, Chuanyong;  Zhao, Longhai;  Li, Pengting
收藏  |  浏览/下载:120/0  |  提交时间:2021/10/15
new Ni-Co-based superalloy  segregations  silicon  solidifications