IMR OpenIR

浏览/检索结果: 共17条,第1-10条 帮助

已选(0)清除 条数/页:   排序方式:
Melting of primary carbides in a cobalt-base superalloy 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 卷号: 787, 页码: 152-157
作者:  Gui, Weimin;  Zhang, Xiaotian;  Zhang, Hongyu;  Sun, Xiaofeng;  Zheng, Qi
收藏  |  浏览/下载:122/0  |  提交时间:2021/02/02
Cobalt-base superalloy  Eutectic carbide  Local melting  Re-solidification  
Influence of type and morphology of carbides on stress-rupture behavior of a cast cobalt-base superalloy 期刊论文
ELSEVIER SCIENCE SA, 2017, 卷号: 728, 页码: 145-151
作者:  Gui, Weimin;  Zhang, Hongyu;  Yang, Min;  Jin, Tao;  Sun, Xiaofeng;  Zheng, Qi;  Zheng, Q (reprint author), Chinese Acad Sci, Inst Met Res, Superalloys Div, 72 Wenhua Rd, Shenyang 110016, Liaoning, Peoples R China.
收藏  |  浏览/下载:170/0  |  提交时间:2018/01/10
Cobalt-base Superalloy  Heat Treatment  Stress-rupture  Carbide  Phase Transformation  
The investigation of carbides evolution in a cobalt-base superalloy at elevated temperature 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 卷号: 695, 页码: 1271-1278
作者:  Gui, Weimin;  Zhang, Hongyu;  Yang, Min;  Jin, Tao;  Sun, Xiaofeng;  Zheng, Qi;  Zheng, Q (reprint author), Chinese Acad Sci, Superalloys Div, Inst Met Res, 72 Wenhua Rd, Shenyang 110016, Peoples R China.
收藏  |  浏览/下载:136/0  |  提交时间:2017/08/17
Cobalt-base Superalloy  M7c3 Decomposition  Mc Degeneration  Microstructure  Heat Treatment  
The isothermal and cyclic oxidation behaviour of two Co modified aluminide coatings at high temperature 期刊论文
Corrosion Science, 2014, 卷号: 84, 页码: 42-53
作者:  Q. X. Fan;  X. Peng;  H. J. Yu;  S. M. Jiang;  J. Gong;  C. Sun
收藏  |  浏览/下载:123/0  |  提交时间:2014/07/03
Metal Coatings  Superalloys  Sem  Xrd  Oxidation  Base Superalloy  Hot Corrosion  Alloying Elements  Nial Alloys  Cobalt  Cr  Metals  Scales  Blade  Al  
The effect of Co on the microstructure and stress rupture properties of a single crystal superalloy 期刊论文
Materials Research Innovations, 2014, 卷号: 18, 页码: 414-420
作者:  J. L.;  Zhang Liu, J.;  Meng, J.;  Jia, Y. X.;  Jin, T.
收藏  |  浏览/下载:96/0  |  提交时间:2015/05/08
Co  Single Crystal Superalloy  Dendrite  Chemical Segregation  Stress  Rupture  Nickel-base Superalloy  Cobalt  
Recrystallization in a directionally solidified cobalt-base superalloy 期刊论文
Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2008, 卷号: 480, 期号: 1-2, 页码: 428-433
作者:  S. Pu;  J. Zhang;  Y. F. Shen;  L. H. Lou
Adobe PDF(1867Kb)  |  收藏  |  浏览/下载:119/0  |  提交时间:2012/04/13
Recrystallization  Cobalt-base Superalloy  Directional Solidification  Carbides  Pinning  Twinning  Single-crystal  Mechanical-properties  Diffusion  Alloys  
Preparation and oxidation behavior of NiCrAlYSi coating on a cobalt-base superalloy K40S 期刊论文
Corrosion Science, 2008, 卷号: 50, 期号: 6, 页码: 1707-1715
作者:  K. Zhang;  Q. M. Wang;  C. Sun;  F. H. Wang
Adobe PDF(1375Kb)  |  收藏  |  浏览/下载:67/0  |  提交时间:2012/04/13
Cobalt-base Superalloy K40s  Nicralysi Coating  Arc Ion Plating  High  Temperature Oxidation  Inter-diffusion  Aluminide Coatings  Cyclic Oxidation  Alloys  
Role of Re and Co on microstructures and gamma ' coarsening in single crystal superalloys 期刊论文
Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2008, 卷号: 479, 期号: 1-2, 页码: 148-156
作者:  W. Z. Wang;  T. Jin;  J. L. Liu;  X. F. Sun;  H. R. Guan;  Z. Q. Hu
Adobe PDF(2451Kb)  |  收藏  |  浏览/下载:97/0  |  提交时间:2012/04/13
Rhenium  Cobalt  Gamma' Coarsening  Tcp Phase  Single Crystal Superalloy  Base Super-alloy  Cobalt  Additions  Mar-m247  Tantalum  Tungsten  Phase  
Fatigue crack propagation behavior of K40S cobalt-base superalloy at elevated temperature 期刊论文
Transactions of Nonferrous Metals Society of China, 2003, 卷号: 13, 期号: 1, 页码: 50-54
作者:  F. M. Yang;  X. F. Sun;  H. R. Guan;  W. L. Deng;  F. Liu;  Z. Q. Hu
收藏  |  浏览/下载:70/0  |  提交时间:2012/04/14
Cobalt-base Superalloy  Fatigue Crack Propagation  Fatigue Threshold  Ductility  Growth-behavior  Alloy  Steel  
Low cycle fatigue behavior of K40S cobaltbase superalloy at elevated temperature - I. Fatigue properties 期刊论文
ACTA METALLURGICA SINICA, 2002, 卷号: 38, 期号: 10, 页码: 1047-1052
作者:  Yang, FM;  Sun, XF;  Guan, HR;  Hu, ZQ
收藏  |  浏览/下载:95/0  |  提交时间:2021/02/02
cobalt-base superalloy  high temperature low cycle fatigue  dislocation