Oxidation behavior of a cast polycrystalline Ni-base superalloy in air: At 900 and 1000 degrees C 期刊论文
OXIDATION OF METALS, 2007, 卷号: 68, 期号: 3-4, 页码: 149-163
作者:  Wei, H.;  Hou, G. C.;  Sun, X. F.;  Guan, H. R.;  Hu, Z. Q.
收藏  |  浏览/下载:91/0  |  提交时间:2021/02/02
cast polycrystalline Ni-base superalloy  oxidation  kinetics  microstructure