Effect of Cooling Rate on Microstructure and Mechanical Properties of K465 Superalloy 期刊论文
JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2009, 卷号: 16, 期号: 6, 页码: 70-74
作者:  Pei Zhongye;  Han Wei;  Zhao Gang;  Chen Xingfu;  Li Juntao;  Tian Yanwen
收藏  |  浏览/下载:104/0  |  提交时间:2021/02/02
NICKEL-BASE SUPERALLOY  POWDER-METALLURGY SUPERALLOY  HEAT-TREATMENT  PRECIPITATION  CREEP  cast superalloy  solution heat treatment  cooling rate  microstructure  mechanical property  
Thermal fatigue behavior of cast nickel base superalloy K445 期刊论文
ACTA METALLURGICA SINICA, 2006, 卷号: 42, 期号: 10, 页码: 1056-1060
作者:  Li Youlin;  Yuan Chao;  Guo Jianting
收藏  |  浏览/下载:84/0  |  提交时间:2021/02/02
cast nickel base superalloy  thermal fatigue  carbide  oxidation at high temperature  
On the creep resistance in cast Ni-base superalloys 期刊论文
ZEITSCHRIFT FUR METALLKUNDE, 2006, 卷号: 97, 期号: 2, 页码: 159-163
作者:  Yuan, C;  Guo, JT
收藏  |  浏览/下载:71/0  |  提交时间:2021/02/02
creep resistance  creep deformation mechanism  cast nickel-base superalloy  
Effect of heat treatment on the microstructure and tensile properties of the cast nickel-base superalloy M963 期刊论文
RARE METAL MATERIALS AND ENGINEERING, 2004, 卷号: 33, 期号: 1, 页码: 23-26
作者:  Yin, FS;  Sun, XF;  Hou, GC;  Qi, Z;  Guan, HR;  Hu, ZQ
收藏  |  浏览/下载:151/0  |  提交时间:2021/02/02
cast nickel-base superalloy  heat treatment  microstructure  ductility  
Solidification behavior of a cast nickel-base superalloy 期刊论文
ACTA METALLURGICA SINICA, 2003, 卷号: 39, 期号: 1, 页码: 27-29
作者:  Sun, XF;  Yin, FS;  Li, JG;  Hou, GC;  Zheng, Q;  Guan, HR;  Hu, ZQ
收藏  |  浏览/下载:95/0  |  提交时间:2021/02/02
cast nickel-base superalloy  solidification  microstructure  DTA  
Solidification behavior of a cast nickel-base superalloy 期刊论文
ACTA METALLURGICA SINICA, 2003, 卷号: 39, 期号: 1, 页码: 27-29
作者:  Sun, XF;  Yin, FS;  Li, JG;  Hou, GC;  Zheng, Q;  Guan, HR;  Hu, ZQ
收藏  |  浏览/下载:145/0  |  提交时间:2021/02/02
cast nickel-base superalloy  solidification  microstructure  DTA  
Resistant stress for creep in cast nickel-base superalloys 期刊论文
ACTA METALLURGICA SINICA, 2002, 卷号: 38, 期号: 11, 页码: 1149-1156
作者:  Yuan, C;  Guo, JT;  Yang, HC
收藏  |  浏览/下载:97/0  |  提交时间:2021/02/02
cast nickel-base superalloy  creep mechanism  resistant stress  
Effect of melt superheating on the morphology of MC carbide in a cast Ni-base superalloy M963 期刊论文
Journal of Wuhan University of Technology-Materials Science Edition, 2002, 卷号: 17, 期号: 3, 页码: 42-45
作者:  F. S. Yin;  X. F. Sun;  C. Yuan;  H. R. Guan;  Z. Q. Hu
收藏  |  浏览/下载:76/0  |  提交时间:2012/04/14
Cast Nickel-base Superalloy  Melt Superheating  Mc Carbide  Differential  Thermal Analysis  
Effect of heat treatment on microstructure and high temperature tensile properties of cast nickel-base superalloy with high W, Mo and Nb contents 期刊论文
Transactions of Nonferrous Metals Society of China, Transactions of Nonferrous Metals Society of China, 2002, 2002, 卷号: 12, 12, 期号: 1, 页码: 83-87, 83-87
作者:  F. S. Yin;  X. F. Sun;  Y. Chao;  H. R. Guan;  Z. Q. Hu
收藏  |  浏览/下载:84/0  |  提交时间:2012/04/14
Cast Nickel Base Superalloy  Cast Nickel Base Superalloy  Mechanical Properties  Mechanical Properties  Microstructure  Microstructure  Heat  Heat  Treatment  Treatment  Creep Resistance  Creep Resistance  Gamma'  Gamma'  
Thermo-mechanical fatigue behavior of cast nickel-based superalloy K417 期刊论文
ACTA METALLURGICA SINICA, 2001, 卷号: 37, 期号: 3, 页码: 267-271
作者:  Liu, F;  Al, SH;  Wang, YC;  Zhang, H;  Wang, ZG
收藏  |  浏览/下载:88/0  |  提交时间:2021/02/02
cast nickel-base superalloy  thermo-mechanical fatigue  in-phase  out-of-phase