IMR OpenIR

浏览/检索结果: 共2条,第1-2条 帮助

已选(0)清除 条数/页:   排序方式:
Corrosion Behavior of Pure Ti under a Solid NaCl Deposit in a Wet Oxygen Flow at 600 degrees C 期刊论文
METALS, 2016, 卷号: 6, 期号: 4
作者:  Fan, Lei;  Liu, Li;  Cao, Min;  Yu, Zhongfen;  Li, Ying;  Chen, Minghui;  Wang, Fuhui;  Liu, L;  Li, Y (reprint author), Chinese Acad Sci, Inst Met Res, Wencui Rd 62, Shenyang 110016, Peoples R China.
收藏  |  浏览/下载:148/0  |  提交时间:2016/08/22
Titanium  Corrosion  Solid Nacl Deposit  Intermediate Temperature  Potentiodynamic Polarization  
Oxidation and H2O/NaCl-induced corrosion behavior of sputtered Ni-Si coatings on Ti6A14V at 600-650 degrees C 期刊论文
Surface & Coatings Technology, 2007, 卷号: 201, 期号: 16-17, 页码: 7530-7537
作者:  C. Z. Yu;  S. L. Zhu;  D. Z. Wei;  F. H. Wang
收藏  |  浏览/下载:98/0  |  提交时间:2012/04/13
Ni-si Coating  Oxidation  Corrosion  Water Vapor  Nacl Deposit  High  Temperature  Solid Nacl Deposit  Plus Water-vapor  Titanium-alloy  Air Oxidation  Composite Coatings  Ti-6al-4v Alloy  Ti6al4v Alloy  Resistance  Cr  Hydrogen