Ultrafast Electrochemical Growth of Lithiophilic Nano-Flake Arrays for Stable Lithium Metal Anode 期刊论文
ADVANCED FUNCTIONAL MATERIALS, 2021, 页码: 10
作者:  Shen, Haorui;  Qi, Fulai;  Li, Hucheng;  Tang, Pei;  Gao, Xuning;  Yang, Shan;  Hu, Zichen;  Li, Zhuangnan;  Tan, Jun;  Bai, Shuo;  Li, Feng
收藏  |  浏览/下载:153/0  |  提交时间:2021/11/22
Cu  S-7  (4) nano-flake arrays  dead lithium  Li  S-2-enriched solid electrolyte interface  lithium dendrites  lithium metal anode  
Ultrafast Electrochemical Growth of Lithiophilic Nano-Flake Arrays for Stable Lithium Metal Anode 期刊论文
ADVANCED FUNCTIONAL MATERIALS, 2021, 页码: 10
作者:  Shen, Haorui;  Qi, Fulai;  Li, Hucheng;  Tang, Pei;  Gao, Xuning;  Yang, Shan;  Hu, Zichen;  Li, Zhuangnan;  Tan, Jun;  Bai, Shuo;  Li, Feng
收藏  |  浏览/下载:214/0  |  提交时间:2021/11/22
Cu  S-7  (4) nano-flake arrays  dead lithium  Li  S-2-enriched solid electrolyte interface  lithium dendrites  lithium metal anode  
Prediction of the S-N curves of high-strength steels in the very high cycle fatigue regime 期刊论文
International Journal of Fatigue, 2010, 卷号: 32, 期号: 8, 页码: 1351-1357
作者:  Y. B. Liu;  Y. D. Li;  S. X. Li;  Z. G. Yang;  S. M. Chen;  W. J. Hui;  Y. Q. Weng
Adobe PDF(542Kb)  |  收藏  |  浏览/下载:123/0  |  提交时间:2012/04/13
Very High Cycle Fatigue (Vhcf)  S-n Curve  Non-metallic Inclusion  High-strength Steel  Chromium-bearing Steel  Long-life Fatigue  Subsurface Crack Initiation  Gigacycle Fatigue  Inclusion Size  N-greater-than-10(7) Cycles  Propagation Behavior  Spring Steel  Part Ii  Failure