Effect of purity on solidification structure and micro-segregation in a nickel-based single crystal superalloy 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 卷号: 999, 页码: 11
作者:  Wang, Yinghao;  Zhang, Xiaoxin;  Tian, Haoxin;  Hao, Long;  Tian, Zhirui;  Meng, Jie;  Birich, Alexander;  Tan, Yi;  Xuan, Weidong;  Ren, Zhongming
收藏  |  浏览/下载:7/0  |  提交时间:2025/04/27
Nickle-based single crystal superalloy  DD98M  High purity  Solidification structure  Micro-segregation