IMR OpenIR

浏览/检索结果: 共121条,第1-10条 帮助

已选(0)清除 条数/页:   排序方式:
The effect of stress state and He concentration on the dislocation loop evolution in Ni superalloy irradiated by Ni plus & He plus dual-beam ions: In-situ TEM observation and MD simulations 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2025, 卷号: 212, 页码: 77-88
作者:  Zhu, Zhenbo;  Qiu, Rongyang;  Chang, Litao;  Ma, Guangcai;  Deng, Huiqiu;  Huang, Hefei
收藏  |  浏览/下载:4/0  |  提交时间:2025/04/27
Nickel -based superalloy  Dual -beam ion irradiation  Helium bubbles  Dislocation loops  In -situ characterization  MD simulation  
The effect of stress state and He concentration on the dislocation loop evolution in Ni superalloy irradiated by Ni plus & He plus dual-beam ions: In-situ TEM observation and MD simulations 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2025, 卷号: 212, 页码: 77-88
作者:  Zhu, Zhenbo;  Qiu, Rongyang;  Chang, Litao;  Ma, Guangcai;  Deng, Huiqiu;  Huang, Hefei
收藏  |  浏览/下载:3/0  |  提交时间:2025/04/27
Nickel -based superalloy  Dual -beam ion irradiation  Helium bubbles  Dislocation loops  In -situ characterization  MD simulation  
The effect of stress state and He concentration on the dislocation loop evolution in Ni superalloy irradiated by Ni plus & He plus dual-beam ions: In-situ TEM observation and MD simulations 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2025, 卷号: 212, 页码: 77-88
作者:  Zhu, Zhenbo;  Qiu, Rongyang;  Chang, Litao;  Ma, Guangcai;  Deng, Huiqiu;  Huang, Hefei
收藏  |  浏览/下载:3/0  |  提交时间:2025/04/27
Nickel -based superalloy  Dual -beam ion irradiation  Helium bubbles  Dislocation loops  In -situ characterization  MD simulation  
The effect of stress state and He concentration on the dislocation loop evolution in Ni superalloy irradiated by Ni plus & He plus dual-beam ions: In-situ TEM observation and MD simulations 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2025, 卷号: 212, 页码: 77-88
作者:  Zhu, Zhenbo;  Qiu, Rongyang;  Chang, Litao;  Ma, Guangcai;  Deng, Huiqiu;  Huang, Hefei
收藏  |  浏览/下载:1/0  |  提交时间:2025/04/27
Nickel -based superalloy  Dual -beam ion irradiation  Helium bubbles  Dislocation loops  In -situ characterization  MD simulation  
Effect of wall thickness on the microstructure and properties of a fourth-generation single crystal superalloy 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 卷号: 1007, 页码: 11
作者:  Jiang, Kuo;  Liu, Jinlai;  Sheng, Naicheng;  Li, Qi;  Fan, Donghan;  Qiu, Keqiang;  Ren, Yinglei;  Li, Jinguo
收藏  |  浏览/下载:5/0  |  提交时间:2025/04/27
Nickel-based superalloy  Wall thickness  Microstructure  Mechanical properties  
Effect of Solution Treatment on Creep Rupture Properties After Long-Term Aging of Nickel-Based Single Crystal Superalloy 期刊论文
RARE METAL MATERIALS AND ENGINEERING, 2024, 卷号: 53, 期号: 11, 页码: 3129-3135
作者:  Wang, Nan;  Liu, Jide;  Zhu, Chongwei;  Zhang, Zhipeng;  Xu, Wei;  Li, Jinguo
收藏  |  浏览/下载:6/0  |  提交时间:2025/04/27
nickel-based single crystal superalloy  long-time aging  heat treatment regime  microstructure  durational properties  
Effect of Solution Treatment on Creep Rupture Properties After Long-Term Aging of Nickel-Based Single Crystal Superalloy 期刊论文
RARE METAL MATERIALS AND ENGINEERING, 2024, 卷号: 53, 期号: 11, 页码: 3129-3135
作者:  Wang, Nan;  Liu, Jide;  Zhu, Chongwei;  Zhang, Zhipeng;  Xu, Wei;  Li, Jinguo
收藏  |  浏览/下载:5/0  |  提交时间:2025/04/27
nickel-based single crystal superalloy  long-time aging  heat treatment regime  microstructure  durational properties  
Effects of Temperature and Secondary Orientations on the Deformation Behavior of Single-Crystal Superalloys 期刊论文
CRYSTALS, 2024, 卷号: 14, 期号: 11, 页码: 15
作者:  Liu, Sujie;  Zong, Cui;  Ma, Guangcai;  Zhao, Yafeng;  Huang, Junjie;  Guo, Yi;  Chen, Xingqiu
收藏  |  浏览/下载:4/0  |  提交时间:2025/04/27
nickel-based superalloy  secondary orientation  quasi in situ EBSD  geometrically necessary dislocations (GNDs)  deformation mechanisms  
Flame-retardant mechanism for platinum coating of nickel-based superalloy 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 卷号: 1002, 页码: 6
作者:  Cao, Shuting;  Zhao, Jian;  Gong, Tongzhao;  Zhang, Shaohua;  Zhang, Jian
收藏  |  浏览/下载:3/0  |  提交时间:2025/04/27
Nickel-based superalloy  Platinum coating  Flammability  Oxygen-enriched atmosphere  
Flame-retardant mechanism for platinum coating of nickel-based superalloy 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 卷号: 1002, 页码: 6
作者:  Cao, Shuting;  Zhao, Jian;  Gong, Tongzhao;  Zhang, Shaohua;  Zhang, Jian
收藏  |  浏览/下载:2/0  |  提交时间:2025/04/27
Nickel-based superalloy  Platinum coating  Flammability  Oxygen-enriched atmosphere