Effect of Solution Treatment on Creep Rupture Properties After Long-Term Aging of Nickel-Based Single Crystal Superalloy 期刊论文
RARE METAL MATERIALS AND ENGINEERING, 2024, 卷号: 53, 期号: 11, 页码: 3129-3135
作者:  Wang, Nan;  Liu, Jide;  Zhu, Chongwei;  Zhang, Zhipeng;  Xu, Wei;  Li, Jinguo
收藏  |  浏览/下载:6/0  |  提交时间:2025/04/27
nickel-based single crystal superalloy  long-time aging  heat treatment regime  microstructure  durational properties  
Effect of Solution Treatment on Creep Rupture Properties After Long-Term Aging of Nickel-Based Single Crystal Superalloy 期刊论文
RARE METAL MATERIALS AND ENGINEERING, 2024, 卷号: 53, 期号: 11, 页码: 3129-3135
作者:  Wang, Nan;  Liu, Jide;  Zhu, Chongwei;  Zhang, Zhipeng;  Xu, Wei;  Li, Jinguo
收藏  |  浏览/下载:6/0  |  提交时间:2025/04/27
nickel-based single crystal superalloy  long-time aging  heat treatment regime  microstructure  durational properties  
Study on the mechanism of γ' phase rafting in a 4th generation nickel-based single crystal superalloy during thermal exposure at high temperatures 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 卷号: 980, 页码: 8
作者:  Liu, Pengcheng;  Zhang, Zhen;  Liu, Xingang;  Gao, Yuting;  Hao, Linghui;  Li, Hui;  Lou, Langhong
收藏  |  浏览/下载:6/0  |  提交时间:2025/04/27
gamma' phase rafting  Thermal exposure  Finite element analysis  Dislocation  Nickel-based single crystal Superalloy  
Study on the mechanism of γ' phase rafting in a 4th generation nickel-based single crystal superalloy during thermal exposure at high temperatures 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 卷号: 980, 页码: 8
作者:  Liu, Pengcheng;  Zhang, Zhen;  Liu, Xingang;  Gao, Yuting;  Hao, Linghui;  Li, Hui;  Lou, Langhong
收藏  |  浏览/下载:5/0  |  提交时间:2025/04/27
gamma' phase rafting  Thermal exposure  Finite element analysis  Dislocation  Nickel-based single crystal Superalloy  
EFFECTS OF TEMPERATURE AND STRAIN AMPLITUDE ON LOW-CYCLE FATIGUE PROPERTIES OF NICKEL-BASED SINGLE-CRYSTAL SUPERALLOY DD419 期刊论文
MATERIALI IN TEHNOLOGIJE, 2024, 卷号: 58, 期号: 5, 页码: 567-575
作者:  Du, Xiaoming;  Dong, Weiye;  Zhu, Xiang;  Liu, Jide;  Wang, Zhijun;  Li, Tianfu
收藏  |  浏览/下载:4/0  |  提交时间:2025/04/27
nickel-based single-crystal superalloy  low-cycle fatigue  temperature  strain  
EFFECTS OF TEMPERATURE AND STRAIN AMPLITUDE ON LOW-CYCLE FATIGUE PROPERTIES OF NICKEL-BASED SINGLE-CRYSTAL SUPERALLOY DD419 期刊论文
MATERIALI IN TEHNOLOGIJE, 2024, 卷号: 58, 期号: 5, 页码: 567-575
作者:  Du, Xiaoming;  Dong, Weiye;  Zhu, Xiang;  Liu, Jide;  Wang, Zhijun;  Li, Tianfu
收藏  |  浏览/下载:3/0  |  提交时间:2025/04/27
nickel-based single-crystal superalloy  low-cycle fatigue  temperature  strain  
Uncovering the high-temperature microstructural evolution and creep-fatigue damage mechanism of CMSX-4 brazed joints 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2023, 卷号: 173, 页码: 14
作者:  Lu, Chuanyang;  Qin, Zhulai;  Wang, Shiyang;  He, Yanming;  Sun, Yuan;  Gao, Zengliang;  Tu, Shan -Tung
收藏  |  浏览/下载:10/0  |  提交时间:2024/01/07
Nickel -based single -crystal superalloy  Brazing  Creep -fatigue  Microstructural evolution  Damage mechanism  
Epitaxial growth and oxidation behavior of the NiCoCrAlYTa/Y2O3 coating on a nickel-based single-crystal superalloy blade tips, produced by electro spark deposition 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 卷号: 931, 页码: 14
作者:  Yang, Shuai;  Gao, Siyang;  Xue, Weihai;  Wu, Bi;  Cheng, Hao;  Duan
收藏  |  浏览/下载:45/0  |  提交时间:2023/05/09
Nickel -based single -crystal superalloy  Blade tip coating  Epitaxial growth  Electro spark deposition  Oxidation resistance  Nanoparticles  
Epitaxial growth and oxidation behavior of the NiCoCrAlYTa/Y2O3 coating on a nickel-based single-crystal superalloy blade tips, produced by electro spark deposition 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 卷号: 931, 页码: 14
作者:  Yang, Shuai;  Gao, Siyang;  Xue, Weihai;  Wu, Bi;  Cheng, Hao;  Duan
收藏  |  浏览/下载:39/0  |  提交时间:2023/05/09
Nickel -based single -crystal superalloy  Blade tip coating  Epitaxial growth  Electro spark deposition  Oxidation resistance  Nanoparticles  
Unveiling the Re effect on long-term coarsening behaviors of ? ' precipitates in Ni-based single crystal superalloys 期刊论文
ACTA MATERIALIA, 2022, 卷号: 233, 页码: 16
作者:  Lu, Fan;  Antonov, Stoichko;  Lu, Song;  Zhang, Jiachen;  Li, Longfei;  Wang, Dong;  Zhang, Jian;  Feng, Qiang
收藏  |  浏览/下载:137/0  |  提交时间:2022/07/14
Nickel-based single crystal superalloy  Rhenium-effect  Long-term thermal exposure  Atom-probe tomography  Coarsening kinetics