Effects of cerium addition on the microstructure and stress rupture properties of a new nickel-based cast superalloy 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2023, 卷号: 159, 页码: 112-124
作者:  Rong, Lirong;  Wang, Min;  Xing, Weiwei;  Hao, Xianchao;  Ma, Yingche
收藏  |  浏览/下载:12/0  |  提交时间:2024/01/07
Nickel -based cast superalloy  Cerium  M C carbide  Stress rupture properties