Portevin-Le Chatelier (PLC) effect induced by different deformation mechanisms in Ni-25Mo-8Cr alloy during high-temperature tensile deformation 期刊论文
RARE METALS, 2024, 页码: 17
作者:  Yang, Ming;  Luo, Tao;  Lei, Lei;  Jiang, Yun;  Wang, Pan-Zhi;  Xu, Fa-Hong
收藏  |  浏览/下载:6/0  |  提交时间:2025/04/27
Ni-Mo-Cr superalloy  Pt2Mo precipitates  PLC effect  Deformation mechanism  
Influence Mechanism of Silicon on Carbide Phase Precipitation of a Corrosion Resistance Nickel Based Superalloy 期刊论文
MATERIALS, 2020, 卷号: 13, 期号: 4, 页码: 24
作者:  Liu, Tao;  Yang, Mei;  Han, Fenfen;  Dong, Jiasheng
收藏  |  浏览/下载:140/0  |  提交时间:2021/02/02
Ni-Mo-Cr based superalloy  silicon  diffusion  carbide  precipitation  
Influence Mechanism of Silicon on Carbide Phase Precipitation of a Corrosion Resistance Nickel Based Superalloy 期刊论文
MATERIALS, 2020, 卷号: 13, 期号: 4, 页码: 24
作者:  Liu, Tao;  Yang, Mei;  Han, Fenfen;  Dong, Jiasheng
收藏  |  浏览/下载:138/0  |  提交时间:2021/02/02
Ni-Mo-Cr based superalloy  silicon  diffusion  carbide  precipitation