Tensile Properties and Deformation Mechanisms of Ni-Co-W Based Superalloy with High γ′ Content 期刊论文
METALS AND MATERIALS INTERNATIONAL, 2024, 页码: 9
作者:  Tai, Wenbin;  Zhang, Rui;  Zhou, Zijian;  Cui, Chuanyong;  Zhou, Yizhou;  Sun, Xiaofeng
收藏  |  浏览/下载:6/0  |  提交时间:2025/04/27
Ni-Co-W based superalloy  Tensile properties  Deformation mechanism  SFs  Microtwins  
Tensile Properties and Deformation Mechanisms of Ni-Co-W Based Superalloy with High γ′ Content 期刊论文