IMR OpenIR

浏览/检索结果: 共13条,第1-10条 帮助

已选(0)清除 条数/页:   排序方式:
Effect of strain rate on microstructure evolution of a fine-grained gamma plus gamma' Ni-Co-base superalloy during superplasticity 期刊论文
MATERIALS CHARACTERIZATION, 2023, 卷号: 203, 页码: 13
作者:  Al-Hammadi, Rashad A.;  Zhang, Rui;  Cui, Chuanyong;  Zhou, Zijian;  Zhou, Yizhou
收藏  |  浏览/下载:13/0  |  提交时间:2024/01/08
Ni-Co-base superalloy  Superplasticity  Microstructure evolution  gamma'-phase  Twin  
Influence of solution temperature on microstructure and creep behaviors of a Ni-Co base superalloy for turbine disc 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 卷号: 853, 页码: 13
作者:  Zhou, Zijian;  Zhang, Rui;  Cui, Chuanyong;  Zhou, Yizhou;  Sun, Xiaofeng
收藏  |  浏览/下载:35/0  |  提交时间:2023/05/09
Ni-Co base Superalloy  Solution temperature  Grain boundary character distribution  Carbide morphology  Creep behavior  
Effect of pre-strain treatment on mechanical properties of a Ni-Co base disk superalloy 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 卷号: 905, 页码: 10
作者:  Zhu, C. Z.;  Zhang, R.;  Cui, C. Y.;  Zhou, Y. Z.;  Qu, J. L.;  Gan, B.;  Zhang, B. J.;  Sun, X. F.
收藏  |  浏览/下载:127/0  |  提交时间:2022/07/01
Ni-Co base superalloy  Pre-strain  Microstructure  Mechanical property  Microtwinning  Suzuki segregation  
Evolution of Interfacial Microstructure of Ni-Co Base Superalloy During Plastic Deformation Bonding and Its Bonding Mechanism 期刊论文
ACTA METALLURGICA SINICA, 2022, 卷号: 58, 期号: 2, 页码: 129-140
作者:  Ren Shaofei;  Zhang Jianyang;  Zhang Xinfang;  Sun Mingyue;  Xu Bin;  Cui Chuanyong
收藏  |  浏览/下载:146/0  |  提交时间:2022/07/01
Ni-Co base superalloy  plastic deformation bonding  dynamic recrystallization  
Influence of Ta content on microstructure and creep behavior of a Ni-Co base disc superalloy 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 卷号: 802, 页码: 10
作者:  Zhu, C. Z.;  Zhang, R.;  Cui, C. Y.;  Zhou, Y. Z.;  Liang, F. G.;  Liu, X.;  Sun, X. F.
收藏  |  浏览/下载:111/0  |  提交时间:2021/10/15
Ni-Co base superalloy  Tantalum  Microstructure  Creep behavior  
Influence of Ta content on microstructure and creep behavior of a Ni-Co base disc superalloy 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 卷号: 802, 页码: 10
作者:  Zhu, C. Z.;  Zhang, R.;  Cui, C. Y.;  Zhou, Y. Z.;  Liang, F. G.;  Liu, X.;  Sun, X. F.
收藏  |  浏览/下载:118/0  |  提交时间:2021/10/15
Ni-Co base superalloy  Tantalum  Microstructure  Creep behavior  
Influence of Co content on the microstructures and mechanical properties of a Ni-Co base superalloy made by specific additive manufacturing process 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 卷号: 786, 页码: 10
作者:  Tang, Ling;  Liang, Jingjing;  Cui, Chuanyong;  Li, Jinguo;  Zhou, Yizhou;  Sun, Xiaofeng;  Ding, Yutian
收藏  |  浏览/下载:140/0  |  提交时间:2021/02/02
Additive manufacturing  Ni-Co base Superalloy  Tensile strength  Deformation mechanism  
Precipitation and phase transformation mechanism of additive manufactured Ni-Co base superalloy 期刊论文
MATERIALS CHARACTERIZATION, 2019, 卷号: 151, 页码: 252-259
作者:  Tang, Ling;  Liang, Jingjing;  Cui, Chuanyong;  Li, Jinguo;  Zhou, Yizhou;  Sun, Xiaofeng;  Ding, Yutian
收藏  |  浏览/下载:133/0  |  提交时间:2021/02/02
Additive manufacturing  Ni-Co base superalloy  eta phase  Element loss  
Microstructural Evolution of a Ni-base Alloy DZ468 Joint Bonded with a New Co-base Filler 期刊论文
Journal of Materials Science & Technology, 2014, 卷号: 30, 期号: 5, 页码: 480-486
作者:  Y. H. Jing;  Z. Zheng;  E. Z. Liu;  Y. Guo
收藏  |  浏览/下载:117/0  |  提交时间:2014/07/03
Transient Liquid Phase (Tlp) Bonding  Microstructure Evolution  Ni-base  Alloy  Co-base Filler  Hot Corrosion-resistance  Transient Liquid-phase  Compressive  Properties  High-strength  Superalloy  Gamma  Cast  
Dynamic Strain Aging in a Newly Developed Ni-Co-Base Superalloy with Low Stacking Fault Energy 期刊论文
Journal of Materials Science & Technology, 2013, 卷号: 29, 期号: 9, 页码: 873-878
作者:  C. G. Tian;  C. Y. Cui;  L. Xu;  Y. F. Gu;  X. F. Sun
收藏  |  浏览/下载:127/0  |  提交时间:2013/12/24
Ni-co Base Superalloy  Dynamic Strain Aging (Dsa)  Activation Energy  Substitutional Solute  Stacking Fault  Serrated Flow  Activation-energy  Mechanical-properties  Rate  Sensitivity  Stress  Temperature  Alloy  Parameters  Model