Effect of strain rate on plastic deformation bonding behavior of Ni-based superalloys 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2020, 卷号: 40, 页码: 54-63
作者:  Zhang, Jian Yang;  Xu, Bin;  Tariq, Naeem ul Haq;  Sun, Ming Yue;  Li, Dian Zhong;  Li, Yi Yi
收藏  |  浏览/下载:120/0  |  提交时间:2021/02/02
Inconel 718 superalloy  Isothermal compression bonding  Dynamic recrystallization  Grain boundary  Subgrain  Strain rate  
Residual Stress Evolution and Its Mechanism During the Manufacture of Superalloy Disk Forgings 期刊论文
ACTA METALLURGICA SINICA, 2019, 卷号: 55, 期号: 9, 页码: 1160-1174
作者:  Bi Zhongnan;  Qin Hailong;  Dong Zhiguo;  Wang Xiangping;  Wang Ming;  Liu Yongquan;  Du Jinhui;  Zhang Ji
收藏  |  浏览/下载:176/0  |  提交时间:2021/02/02
TEMPERATURE STRUCTURE STABILITY  SITU NEUTRON-DIFFRACTION  IN-SITU  SINGLE-CRYSTAL  CREEP-BEHAVIOR  TURBINE DISC  INCONEL 718  RELAXATION  MICROSTRUCTURE  DISTORTION  superalloy  residual stress  neutron diffraction  contour method  turbine disk  
Tool wear performance and surface integrity studies for milling DD5 Ni-based single crystal superalloy 期刊论文
SCIENCE CHINA-TECHNOLOGICAL SCIENCES, 2018, 卷号: 61, 期号: 4, 页码: 522-534
作者:  Gong, YD;  Li, Q;  Li, JG;  Liu, Y;  Sun, Y;  Gong, YD (reprint author), Northeastern Univ, Sch Mech Engn & Automat, Shenyang 110819, Liaoning, Peoples R China.
收藏  |  浏览/下载:138/0  |  提交时间:2018/06/05
Minimum Quantity Lubrication  Nickel-based Superalloy  Inconel 718  Cutting Forces  Alloys  Dry  Mechanisms  Life  
Preparation of hot-isostatic-pressed powder metallurgy superalloy Inconel 718 free of prior particle boundaries 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 卷号: 682, 页码: 341-344
作者:  Chang, Litao;  Sun, Wenru;  Cui, Yuyou;  Yang, Rui;  Yang, R (reprint author), Chinese Acad Sci, Inst Met Res, Shenyang 110016, Peoples R China.
收藏  |  浏览/下载:128/0  |  提交时间:2017/08/17
Superalloy  Powder Metallurgy  Hot Isostatic Pressing  Prior Particle Boundary  Inconel 718  
Effect of heat treatment on microstructure and mechanical properties of the hot-isostatic-pressed Inconel 718 powder compact 期刊论文
Journal of Alloys and Compounds, 2014, 卷号: 590, 页码: 227-232
作者:  L. T. Chang;  W. R. Sun;  Y. Y. Cui;  F. Q. Zhang;  R. Yang
收藏  |  浏览/下载:133/0  |  提交时间:2014/03/14
Superalloy  Inconel 718  Hot Isostatic Pressing  Heat Treatment  Gamma  '' Precipitation  Ductility  Superalloy Inconel-718  Precipitation  Alloy  
Influence of deformation level on microstructure and creep behavior of GH4169 alloy 期刊论文
Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2012, 卷号: 550, 页码: 235-242
作者:  S. G. Tian;  Z. R. Li;  Z. G. Zhao;  L. Q. Chen;  W. R. Sun;  X. H. Liu
收藏  |  浏览/下载:93/0  |  提交时间:2013/02/05
Gh4169 Alloy  Hot Continuous Rolling  Microstructure  Creep  Deformation  Mechanism  Intermediate Temperature  Inconel 718  Superalloy  Mechanisms  
Segregation and diffusion behavior of niobium in a highly alloyed nickel-base superalloy 期刊论文
Transactions of Nonferrous Metals Society of China, 2011, 卷号: 21, 期号: 11, 页码: 2402-2407
作者:  X. L. Pan;  H. Y. Yu;  G. F. Tu;  W. R. Sun;  Z. Q. Hu
Adobe PDF(1501Kb)  |  收藏  |  浏览/下载:85/0  |  提交时间:2012/04/13
Gh742y Superalloy  Niobium  Segregation  Diffusion  Directionally Solidified Superalloy  Inconel-718 Alloy  Microstructure  Homogenization  Gamma'  
Hot die forging process optimization of superalloy IN718 turbine disc using processing map and finite element method 期刊论文
Proceedings of the Institution of Mechanical Engineers Part B-Journal of Engineering Manufacture, 2010, 卷号: 224, 期号: B1, 页码: 103-110
作者:  H. Y. Zhang;  S. H. Zhang;  Z. X. Li;  M. Cheng
Adobe PDF(446Kb)  |  收藏  |  浏览/下载:94/0  |  提交时间:2012/04/13
Superalloy In718  Turbine Disc  Processing Map  Finite Element Method  Microstructure Simulation  High-temperature Deformation  Metadynamic Recrystallization  Microstructural Evolution  Flow Behavior  Inconel-718  Working  Simulation  In-718  
High temperature low cycle fatigue behavior of a directionally solidified Ni-base superalloy DZ951 期刊论文
Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2008, 卷号: 488, 期号: 1-2, 页码: 389-397
作者:  Z. K. Chu;  J. J. Yu;  X. F. Sun;  H. R. Guan;  Z. Q. Hu
Adobe PDF(2209Kb)  |  收藏  |  浏览/下载:76/0  |  提交时间:2012/04/13
Nickel-base Superalloy  Low Cycle Fatigue  Cyclic Deformation  Cyclic  Stress Response  Nimonic Pe-16 Superalloy  Room-temperature  Crystallographic  Orientation  Inconel 718  Strain-rate  Deformation  Mechanisms  Property  Fracture  Tensile  
Effect of temperature and strain amplitude on dislocation structure of M963 superalloy during high-temperature low cycle fatigue 期刊论文
Materials Transactions, 2006, 卷号: 47, 期号: 1, 页码: 67-71
作者:  L. Z. He;  Q. Zheng;  X. F. Sun;  H. R. Guan;  Z. Q. Hu;  K. Tieu;  C. Lu;  H. T. Zhu
收藏  |  浏览/下载:93/0  |  提交时间:2012/04/13
M963 Superalloy  Low Cycle Fatigue (Lcf)  Temperature  Strain Amplitude  Dislocation Structure  Ni-base Superalloy  Single-crystal Superalloy  Crystallographic  Orientation  Deformation-behavior  In-100 Superalloy  Room-temperature  Stainless-steel  Inconel 718  Creep  Morphology