Evolution and mechanism of recrystallization microstructure and texture in GH3536 superalloy foil and their influence on strength performance 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 卷号: 913, 页码: 14
作者:  Cui, Junjun;  Zhao, Mingjiu;  Jiang, Haichang;  Rong, Lijian;  Wang, Yitong
收藏  |  浏览/下载:2/0  |  提交时间:2025/04/27
GH3536 superalloy foil  Secondary recrystallization  Recrystallization texture  Cold-rolled process  Grain size  Strength performance