Primary carbide evolution and homogenization behavior of a novel Fe-Ni-based superalloy for advanced nuclear reactor 期刊论文
MATERIALS CHARACTERIZATION, 2025, 卷号: 221, 页码: 13
作者:  Wu, Jinrong;  Wang, Jiaqi;  Zhao, Zhipeng;  Guan, Xianjun;  Wu, Yunsheng;  Qin, Xuezhi;  Zhou, Lanzhang
收藏  |  浏览/下载:7/0  |  提交时间:2025/04/27
MC carbides  Fe-Ni-based superalloy  Homogenization  Diffusion kinetics  
Tailoring microstructural stability and stress rupture properties of a solid-solution strengthened Fe-Ni-based superalloy via niobium addition 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 卷号: 1008, 页码: 15
作者:  Wang, J. Q.;  Wu, J. R.;  Guan, X. J.;  Wu, Y. S.;  Cheng, S. H.;  Qin, X. Z.;  Zhou, L. Z.
收藏  |  浏览/下载:5/0  |  提交时间:2025/04/27
Fe-Ni-based superalloy  Niobium  Microstructural stability  Stress rupture properties  Precipitates  
Tailoring microstructural stability and stress rupture properties of a solid-solution strengthened Fe-Ni-based superalloy via niobium addition 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 卷号: 1008, 页码: 15
作者:  Wang, J. Q.;  Wu, J. R.;  Guan, X. J.;  Wu, Y. S.;  Cheng, S. H.;  Qin, X. Z.;  Zhou, L. Z.
收藏  |  浏览/下载:9/0  |  提交时间:2025/04/27
Fe-Ni-based superalloy  Niobium  Microstructural stability  Stress rupture properties  Precipitates  
Effect of PWHT on microstructure and mechanical properties of welded joint of a new Fe-Ni-based superalloy 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 卷号: 906, 页码: 14
作者:  Huang, Yeshun;  Zhang, Rui;  Wang, Fuqiang;  Zhou, Zijian;  Zhang, Peng;  Yan, Jingbo;  Yuan, Yong;  Gu, Yuefeng;  Cui, Chuanyong;  Zhou, Yizhou;  Sun, Xiaofeng
收藏  |  浏览/下载:6/0  |  提交时间:2025/04/27
Fe-Ni-based superalloy  Post weld heat treatment  Tensile behavior  Stress relaxation cracking  Creep properties  
Influence of γ′ precipitate on impact toughness and tensile properties of a new Fe-Ni-based superalloy 期刊论文
INTERMETALLICS, 2024, 卷号: 166, 页码: 9
作者:  Huang, Yeshun;  Zhang, Rui;  Zhou, Zijian;  Zhang, Peng;  Yan, Jingbo;  Yuan, Yong;  Gu, Yuefeng;  Cui, Chuanyong;  Zhou, Yizhou;  Sun, Xiaofeng
收藏  |  浏览/下载:3/0  |  提交时间:2025/04/27
Fe-Ni-based superalloy  gamma ' precipitate  Impact toughness  Tensile behavior  
Effects of Al and Ti on thermal expansion behavior of a Ni-Fe-Cr-based superalloy: A combined experimental and first-principle study 期刊论文
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 卷号: 29, 页码: 3805-3812
作者:  Cheng, Sihan;  Qin, Xuezhi;  Wen, Bin;  Wang, Jiaqi;  Wu, Yunsheng;  Zhou, Lanzhang
收藏  |  浏览/下载:6/0  |  提交时间:2025/04/27
Ni-Fe-Cr-based superalloy  Thermal expansion  Microstructure  First -principles  Aluminium  Titanium  
The microstructure and mechanical performance optimization of a new Fe-Ni-based superalloy for Gen IV nuclear reactor: The critical role of Nb alloying strategy 期刊论文
MATERIALS CHARACTERIZATION, 2023, 卷号: 205, 页码: 15
作者:  Wang, Jiaqi;  Qin, Xuezhi;  Cheng, Sihan;  Guan, Xianjun;  Zhou, Lanzhang
收藏  |  浏览/下载:13/0  |  提交时间:2024/01/07
Fe -Ni -based superalloy  Nb alloying  Thermal stability  Tensile property  Deformation mechanism  
Effect of cold rolling on microstructure, texture, and tensile properties of a Ni-Fe-based superalloy 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 卷号: 937, 页码: 14
作者:  Wang, Jiaqi;  Cheng, Sihan;  Wu, Yunsheng;  Wang, Tingting;  Qin, Xuezhi;  Zhou, Lanzhang
收藏  |  浏览/下载:57/0  |  提交时间:2023/05/09
Ni-Fe-based superalloy  Cold rolling  Microstructure  Texture  Strength  Deformation twinning  
Microstructure, thermal stability and tensile properties of a Ni-Fe-Cr based superalloy with different Fe contents 期刊论文
INTERMETALLICS, 2023, 卷号: 153, 页码: 12
作者:  Cheng, Sihan;  Wang, Jiaqi;  Wu, Yunsheng;  Qin, Xuezhi;  Zhou, Lanzhang
收藏  |  浏览/下载:36/0  |  提交时间:2023/05/09
Ni-Fe-Cr based superalloy  Fe content  Microstructure  Thermal exposure  Tensile behavior  
Coherent precipitation and stability of cuboidal B2 nanoparticles in a ferritic Fe-Cr-Ni-Al superalloy 期刊论文
MATERIALS RESEARCH LETTERS, 2021, 卷号: 9, 期号: 11, 页码: 458-466
作者:  Wang, Zhenhua;  Wang, Qing;  Niu, Ben;  Dong, Chuang;  Zhang, Hongwei;  Zhang, Haifeng;  Liaw, Peter K.
收藏  |  浏览/下载:152/0  |  提交时间:2021/11/22
Fe-based superalloy  coherent precipitation  lattice misfit  particle coarsening  mechanical properties