Effects of B and P on Microstructure and Mechanical Properties of a Superalloy Used for 700 degrees C Advanced Ultra-Supercritical Steam Turbine 期刊论文
RARE METAL MATERIALS AND ENGINEERING, 2017, 卷号: 46, 期号: 4, 页码: 1136-1142
作者:  Xiao Xuan;  Yang Cheng;  Qin Xuezhi;  Zhou Yanwen;  Guo Jianting;  Zhou Lanzhang
收藏  |  浏览/下载:124/0  |  提交时间:2021/02/02
700 degrees C advanced ultra-supercritical  Ni-Fe base superalloy  B (boron)  P (phosphorus)  microstructure  mechanical property  
Effects of B and P on Microstructure and Mechanical Properties of a Superalloy Used for 700 degrees C Advanced Ultra-Supercritical Steam Turbine 期刊论文
RARE METAL MATERIALS AND ENGINEERING, 2017, 卷号: 46, 期号: 4, 页码: 1136-1142
作者:  Xiao Xuan;  Yang Cheng;  Qin Xuezhi;  Zhou Yanwen;  Guo Jianting;  Zhou Lanzhang
收藏  |  浏览/下载:120/0  |  提交时间:2021/02/02
700 degrees C advanced ultra-supercritical  Ni-Fe base superalloy  B (boron)  P (phosphorus)  microstructure  mechanical property  
Thermal Stability of a New Ni-Fe-Cr Base Alloy with Different Ti/Al Ratios 期刊论文
Journal of Materials Science & Technology, 2015, 卷号: 31, 期号: 2, 页码: 135-142
作者:  C. S.;  Wang Wang, T. T.;  Tan, M. L.;  Guo, Y. G.;  Guo, J. T.;  Zhou, L. Z.
收藏  |  浏览/下载:149/0  |  提交时间:2015/05/08
700 Degrees c A-usc  Ni-fe-cr Base Alloy  Thermal Stability  Eta Phase  Ti/al Ratio  Nickel-based Superalloy  Coal Power-plants  Mechanical-properties  Eta-phase  Microstructure  
A superheater tube superalloy GH2984 with excellent properties 期刊论文
ACTA METALLURGICA SINICA, 2005, 卷号: 41, 期号: 11, 页码: 1221-1227
作者:  Guo, JT;  Du, XK
收藏  |  浏览/下载:128/0  |  提交时间:2021/02/02
Fe base superalloy  superheater material  mechanical property  microstructure  thermal stability