Influence of Pre-oxidation on the Hot Corrosion of DZ68 Superalloy in the Mixture of Na2SO4-NaCl 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2010, 卷号: 26, 期号: 10, 页码: 895-899
作者:  Liu, Enze;  Zheng, Zhi;  Guan, Xiurong;  Tong, Jian;  Ning, Likui;  Yu, Yongsi
收藏  |  浏览/下载:79/0  |  提交时间:2021/02/02
DZ68 superalloy  Pre-oxidation  Hot corrosion  
Influence of Pre-oxidation on the Hot Corrosion of DZ68 Superalloy in the Mixture of Na(2)SO(4)-NaCl 期刊论文
Journal of Materials Science & Technology, 2010, 卷号: 26, 期号: 10, 页码: 895-899
作者:  E. Z. Liu;  Z. Zheng;  X. R. Guan;  J. A. Tong;  L. K. Ning;  Y. S. Yu
Adobe PDF(514Kb)  |  收藏  |  浏览/下载:80/0  |  提交时间:2012/04/13
Dz68 Superalloy  Pre-oxidation  Hot Corrosion  Ni-based Superalloy  Resistance  Behavior  
STUDY ON HOT CORROSION RESISTANCE OF A NEW DIRECTIONAL SOLIDIFICATION Ni-BASED SUPERALLOY 期刊论文
ACTA METALLURGICA SINICA, 2009, 卷号: 45, 期号: 2, 页码: 161-166
作者:  Ning Likui;  Zheng Zhi;  Tan Yi;  Liu Enze;  Tong Jian;  Yu Yongsi;  Wang Hua
收藏  |  浏览/下载:77/0  |  提交时间:2021/02/02
DZ68  hot corrosion  superalloy