摘要The internal oxidation technology of Al in Cu-Al pre-alloyed powders is discussed. The results show that the reacting temperature is a key factor to determine the critical oxygen partial pressure. The maximum oxygen partial pressure increases with increasing temperature, so that a little higher temperature than that of ordinary reaction is helpful to reduce the difficulty of controlling internal oxidation. High energy milling has little influence on the internal oxidation thermodynamics, however, remarkable influence on the internal oxidation kinetics. When the Al content exceeds 0.5%, the heating parameters should be alternated based on Al content. It can be observed from the examinations of the samples that the spherical Al2O3 particles with an average diameter size of 2-5 mum and particles spacing of 5-10 mum are dispersed in the Cu matrix uniformly, when used the suitable processing parameters of internal oxidation.
关键词Cu-Al pre-alloyed powders internal oxidation high energy milling Al2O3/Cu composite
收录类别SCI
语种英语
WOS研究方向Metallurgy & Metallurgical Engineering
WOS类目Metallurgy & Metallurgical Engineering
WOS记录号WOS:000220611700017
出版者SCIENCE CHINA PRESS
引用统计
被引频次:3[WOS]   [WOS记录]     [WOS相关记录]
文献类型期刊论文
条目标识符http://ir.imr.ac.cn/handle/321006/118432
专题中国科学院金属研究所
通讯作者Liang, SH
作者单位1.Xian Jiaotong Univ, State Key Lab Mech Behav Mat, Xian 710049, Peoples R China
2.Xian Univ Technol, Sch Mat Sci & Engn, Xian 710048, Peoples R China
3.Chinese Acad Sci, Inst Met Res, Shenyang 110016, Peoples R China
推荐引用方式
GB/T 7714
Liang, SH,Xu, L,Fang, L,et al. Analysis on internal oxidation technology of Al in Cu-Al pre-alloyed powders[J]. ACTA METALLURGICA SINICA,2004,40(3):309-313.
APA Liang, SH,Xu, L,Fang, L,&Fan, ZK.(2004).Analysis on internal oxidation technology of Al in Cu-Al pre-alloyed powders.ACTA METALLURGICA SINICA,40(3),309-313.
MLA Liang, SH,et al."Analysis on internal oxidation technology of Al in Cu-Al pre-alloyed powders".ACTA METALLURGICA SINICA 40.3(2004):309-313.
条目包含的文件
条目无相关文件。
个性服务
推荐该条目
保存到收藏夹
查看访问统计
导出为Endnote文件
谷歌学术
谷歌学术中相似的文章
[Liang, SH]的文章
[Xu, L]的文章
[Fang, L]的文章
百度学术
百度学术中相似的文章
[Liang, SH]的文章
[Xu, L]的文章
[Fang, L]的文章
必应学术
必应学术中相似的文章
[Liang, SH]的文章
[Xu, L]的文章
[Fang, L]的文章
相关权益政策
暂无数据
收藏/分享
所有评论 (0)
暂无评论
 

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。